this post was submitted on 07 Jul 2023
9 points (100.0% liked)

3DPrinting

15577 readers
70 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: !functionalprint@kbin.social or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe/ may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
 

I'm printing TPU with .8 mm nozzle and having troubles with the first layer. There are gaps between the layer lines and it looks pretty bumpy.

I'm printing with .3 mm layer height and my print speeds are at 20 mm/s.

Any idea what I could do to improve the first layer?

you are viewing a single comment's thread
view the rest of the comments
[–] MeltedManufacturing@lemmy.world 3 points 1 year ago (1 children)

I think you're right! It's extremely humid right now and when I print I'm hearing snaps and crackles. I'm guessing that is the moisture from the filament?

Thanks for the help!

[–] NiyaShy@kbin.social 4 points 1 year ago

If you can already hear it during normal printing, then yes, it's most likely wet filament. The water trapped inside almost instantly turns into steam inside the nozzle and expands, causing the molten filament to bubble up as the steam escapes.