3DPrinting
3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.
The r/functionalprint community is now located at: !functionalprint@kbin.social or !functionalprint@fedia.io
There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml
Rules
-
No bigotry - including racism, sexism, ableism, homophobia, transphobia, or xenophobia. Code of Conduct.
-
Be respectful, especially when disagreeing. Everyone should feel welcome here.
-
No porn (NSFW prints are acceptable but must be marked NSFW)
-
No Ads / Spamming / Guerrilla Marketing
-
Do not create links to reddit
-
If you see an issue please flag it
-
No guns
-
No injury gore posts
If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)
Moderation policy: Light, mostly invisible
view the rest of the comments
100% agree with adding a coating agent after printing, but if you’re looking to minimize small holes and fissures, consistent line width is super important. High speeds can make thinner lines than when it slows down at starts/stops and corners.
Printing PETG slower than PLA is already a common recommendation, but unless your printer supports input shaping and linear (or pressure) advance, I’d go as slow as you can bear. As a perk, if 245 is the optimal temp for your usual speed, going slower will make 240 work better.
I'm not sure what my optimal temp is yet, I've been using 245 because it was the middle of the range recommended by my filament. I will definitely try slower, I had already slowed to 50% my PLA speed. I'll try like 30% though!