this post was submitted on 06 Jul 2023
26 points (100.0% liked)

3DPrinting

15276 readers
131 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: !functionalprint@kbin.social or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
 

I'm pretty new to PETG, and have been really struggling with it compared to PLA. My latest print of this part is dimensionally accurate, but I need it to be air tight. It is very much not at the moment.

I have a Flashforge Adventurer 3, so the hot end and nozzle are one interchangeable unit. My higher temp nozzle is 0.6mm. My 0.3mm is only capable of 240. My last print was 0.2mm layers, with the 0.6mm nozzle at 245C. I used 15% overlap on my walls, and in order to keep my nice dimensions I had my cooling fan on.

Anybody have any advice on how to improve the seal? I'm tempted to try more overlap, with random start locations per layer. Do you think if I run it hotter I can get the layers a little thinner? Any advice would be appreciated.

you are viewing a single comment's thread
view the rest of the comments
[–] BoxOfFeet@lemmy.world 1 points 1 year ago

Yeah, I will definitely try smaller layer height. The wall thickness is only about 4 or 5 perimeters wide at the thickest point, though. So, I can't really increase that I'm afraid.