3DPrinting
3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.
The r/functionalprint community is now located at: !functionalprint@kbin.social or !functionalprint@fedia.io
There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml
Rules
-
No bigotry - including racism, sexism, ableism, homophobia, transphobia, or xenophobia. Code of Conduct.
-
Be respectful, especially when disagreeing. Everyone should feel welcome here.
-
No porn (NSFW prints are acceptable but must be marked NSFW)
-
No Ads / Spamming / Guerrilla Marketing
-
Do not create links to reddit
-
If you see an issue please flag it
-
No guns
-
No injury gore posts
If you need an easy way to host pictures, https://catbox.moe/ may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)
Moderation policy: Light, mostly invisible
view the rest of the comments
I've definitely noticed less shininess than the same filament was getting at the same temperatures on my previous printer, except for the first layer. As the first layer prints without part cooling, my guess is that the extra part cooling versus the other printer means it's setting before it's had time to self-level. If that's right, then turning down the part cooling (and then also the speed so you can get away with the reduced part cooling) would make things shiny again. I've not bothered investigating that, as most of what I print is either functional, where I wouldn't care about shininess, or gets painted, where any shininess would come from paint or clearcoat.